Compact Grade Laminates

Available in thickness from 3mm to 20 mm. Recommended for application where in mechanical strength, Impact resistance,resistance to water, humidity & heat are the key factors.

Download Catalogue

USPs

Easy to install

Good machinability

Easy maintenance

Excellent stain resistance

Water Resistant

Cost Effective

SR NOPROPERTIES AS PER DIN EN 438 Part 4: 2016Type CGSTEST METHODS AS PER DIN EN 438 Part 2&4: 2016UNITMIN/MAX REQUIREMENT
1ThicknessEN 438-4-6.3mm8.0+/-0.508.0mm+/-0.50
2Resistance to surface wearEN 438-2-10Revolutions (min)150175
3Resistance to immersion in Boiling WaterEN 438-2-12AppearanceRating (min)Gloss Finish - 3, Other Finish - 4
4Resistance to dry Heat at 180°CEN 438-2-16AppearanceRating (min)Gloss Finish - 3, Other Finish - 4
5Dimensional Stability at elevated temperature (Cumulative dimensional change)EN 438-2-17% MaxL: 0.30, T: 0.60L: 0.16, T: 0.28
6Resistance to impact by Large diameter ballEN 438-2-21mm (min)18001900
7Resistance to scratchingEN 438-2-25Rating (min)Smooth finish - 2, Textured finish - 3Smooth finish - ≥ 2, Textured finish - ≥ 3
8Resistance to staining Group 1 & 2, Group 3EN 438-2-26Appearance Rating (min)5, 45, ≥ 4
9Resistance to color change in Xenon Arc light (Light fastness)EN 438-2-27Grey scale rating4 to 5≥ 4
10Resistance to wet heat (100°C)EN12721:1997AppearanceRating (min)Gloss Finish - 3, Other Finish - 4
11Flexural ModulusEN TSO178:2003Mpa900010,000
12Flexural strengthEN TSO178:2003Mpa80110
13DensityEN ISO 1183:1987g/cm3(min)1.351.38

Applications

Home & Office Furniture

Wall Panelling

Wardrobes & Closet Interiors

Office Partitions & Shelves

Hotels & Restaurants

Kitchen Countertops & Backsplashes

Gallery

Heat

Although laminates are tested to a temperature of 180 degrees care should be taken to avoid prolonged exposure to high temperatures. Objects such as oven-hot pans and dishes should not be taken from direct heat and placed directly on the laminate. Burning cigarettes should never be left on the surface. This information will assist in ensuring that surfaces faced with poly grey high-pressure decorative laminate will give good service for many years.

Polish

Polish should not be applied to the surfaces, since it can lead to smearing and marking,particularly on horizontal surfaces.

Scratching

Scraping with sharp edges should be avoided and objects with rough or uneven bases can cause scratches if allowed to slide across the surface. Food should not be chopped on a working surface; the use of a chopping board will prevent permanent damage.

Cleaning

Wipe with a damp cloth or a cloth dipped in mild detergent and water. Clean with washing powder or bleach.Use a melamine sponge with water and wipe but do not scrub too heavily, as that can cause changes in the sheen of HPL products.Remove with an organic solvent such as methylated spirits, acetone, benzene, and nail varnish remover.